Graphite Sagger Generation 2 for Cathode & Anode Materials: 1500°C Secondary Sintering
I. Application Fields
4.5th Generation Lithium Iron Phosphate (LFP) Cathode Materials, Graphite Anode Materials, and Other Oxygen-Free Sintering Applications
II. Operating Temperature Range





1000-3000°C
III. Chemical Composition & Physical Properties
| Category |
Component |
Parameter |
| Chemical Composition |
Carbon Content |
≥99.9% |
| Physical Properties |
Bulk Density |
1.78-1.8 g/cm³ |
| Flexural Strength |
30-40 Mpa |
| Compressive Strength |
≥80 Mpa |
| Antioxidant Performance |
Excellent |
| Thermal Conductivity |
Superior |
| Thermal Shock Resistance (Above 1100°C) |
Excellent |
IV. Product Advantages
- With a carbon content of ≥99.9%, high density, excellent mechanical strength and strong chemical stability, it fundamentally eliminates contamination of the sintered materials.
- Featuring an upgraded antioxidant formula and proprietary secondary sintering process, it delivers significantly enhanced corrosion resistance and high-temperature oxidation resistance, with a service life further extended compared to the first-generation products.
- Optimized thermal performance: It combines excellent thermal conductivity with outstanding thermal shock resistance, enabling uniform heat transfer, ensuring consistent sintering process results and minimizing performance variations between production batches.